Solutions
Horse Construction business range tend to all over the world and service for thousands clients with products, technical,construction specialized guidance, and we witness the Chinese reinfocing brand's togther with them.
Normal carbon fiber fabric pull-out test tensile strength > 2.5 MPa, greater than this data is recognized as the carbon fiber fabric test qualified!
The carbon fiber fabric drawing test can be done on the 3 day after the carbon fiber sample is solidified. Generally, the experimental mold of the drawing instrument is bonded with adhesive, and the curing can be completed in 30 minutes, and the next step can be carried out.
Cutting and separating carbon fiber specimen edge and carbon fiber fabric by cutting machine.
Install the drawing instrument and fix the base and the original structure wall.
After drawing, the concrete thickness of the broken ring interface is about 2~4mm, which basically shows that the experiment is qualified.
The failure of the original concrete section.
Normal carbon fiber fabric pull-out test tensile strength > 2.5 MPa, greater than this data is recognized as the carbon fiber fabric test qualified!
You can find anything here you are in need of, have a trust trying on these products, you will find the big difference after that.
Part A (Epoxy): 20kg
Part B (Hardener): 10kg
Mix Ratio: Part A: Part B=2:1
Consumption Ratio: 6-7kg/sqm
Bar
Part A (Epoxy): 20kg
Part B(Hardener):10kg
Mix Ratio: Part A: Part B=2:1
Barrel A Size: 30*30*37cm
Bar
Part A (Epoxy): 20kg
Part B (Hardener): 10kg
Mix Ratio: Part A: Part B=2:1
Barrel A Size: 30*30*37cm
Barrel B Size: 25*25